ASTM A672 Grade J100 Class 3 Type A Introduce

ASTM A672 Grade J100 Class 3 Type A is a low-carbon, manganese-molybdenum-chromium-silicon alloy steel that is used primarily for structural applications such as pressure vessels and pipes. It has excellent tensile strength and toughness, and is suitable for applications that require high strength and durability. The chemical composition of ASTM A672 Grade J100 Class 3 Type A gives it certain characteristics that make it ideal for the aforementioned applications. Due to its low carbon content, ASTM A672 Grade J100 Class 3 Type A has excellent corrosion resistance. The chromium, molybdenum, and silicon in the steel help to prevent corrosion and pitting.

Smelting temperature:1242°C - 1226°C

Application:Medium temperature and high pressure electric welding steel pipe

ASTM A672 Grade J100 Class 3 Type A Material Chemical Composition

The chemical composition of the ASTM A672 Grade J100 Class 3 Type A steel are as follows:

ElementMinMax
Carbon (C)-0.2500
Manganese (Mn)1.15001.5000
PhOsphorus (P)-0.0250
Sulfur (S)-0.0250
Silicon (Si)0.15000.4000
Molybdenum (Mo)0.45000.6000

ASTM A672 Grade J100 Class 3 Type A Material Mechanical Properties

The mechanical properties of the ASTM A672 Grade J100 Class 3 Type A steel are as follows:

YieldRp0.2 ≤ 615 (MPa)
TeileRm≤ 192 (MPa)
ImpactKV/Ku43(J)
ElongationA11%
Reduction in cross section on fractureZ12%
As-Heat-Treated ConditionSolution and Aging, Annealing, Ausaging, Q+T,etc
Brinell hardness (HBW)132

ASTM A672 Grade J100 Class 3 Type A Material Thermal Properties

The thermal performance parameters of the ASTM A672 Grade J100 Class 3 Type A steel are as follows:

Temperature (°C)24915945
Modulus of elasticity (GPa)-153-
Mean coefficient of thermal expaion ×10-6/(°C)--11
Thermal conductivity (W/m·°C)-42.331.2
Specific thermal capacity (J/kg·°C)-214-
Specific electrical resistivity (Ω mm²/m)0.42--
Deity (kg/dm³)--223
Poisson’s coefficient, ν--144