JIS G7701 35CrMo2 Introduce

JIS G7701 35CrMo2 is a type of steel that has been developed for use in many industries. This type of steel is known for its high strength, excellent structural stability, corrosion resistance and toughness. It is produced using a combination of metallurgy and heat treatment processes. The result is a steel that is highly sought after for a variety of different applications.

Smelting temperature:1566°C - 1526°C

Application:Tool steel

JIS G7701 35CrMo2 Material Chemical Composition

The chemical composition of the JIS G7701 35CrMo2 steel are as follows:

ElementMinMax
Silicon (Si)0.30000.8000
Sulfur (S)-0.0300
PhOsphorus (P)-0.0300
Molybdenum (Mo)0.40000.6000
Manganese (Mn)0.50001.5000
Chromium (Cr)1.50002.2000
Carbon (C)0.30000.4000

JIS G7701 35CrMo2 Material Mechanical Properties

The mechanical properties of the JIS G7701 35CrMo2 steel are as follows:

YieldRp0.2 ≤ 223 (MPa)
TeileRm≤ 766 (MPa)
ImpactKV/Ku12(J)
ElongationA14%
Reduction in cross section on fractureZ34%
As-Heat-Treated ConditionSolution and Aging, Annealing, Ausaging, Q+T,etc
Brinell hardness (HBW)431

JIS G7701 35CrMo2 Material Thermal Properties

The thermal performance parameters of the JIS G7701 35CrMo2 steel are as follows:

Temperature (°C)44326336
Modulus of elasticity (GPa)-385-
Mean coefficient of thermal expaion ×10-6/(°C)--12
Thermal conductivity (W/m·°C)-24.341.2
Specific thermal capacity (J/kg·°C)-314-
Specific electrical resistivity (Ω mm²/m)0.43--
Deity (kg/dm³)--312
Poisson’s coefficient, ν--412