GB/T 1299 T20102 Introduce

The maximum allowable concentrations of phosphorus and sulfur in GB/T 1299 T20102 steel are 0.045%. These elements are often found in low concentrations in alloy steels, as they can have detrimental effects on the performance of the material. Too much phosphorus or sulfur can lead to brittleness or a decrease in ductility.

Smelting temperature:1921°C - 1929°C

Application:Alloy tool steel

GB/T 1299 T20102 Material Chemical Composition

The chemical composition of the GB/T 1299 T20102 steel are as follows:

ElementMinMax
Silicon (Si)0.25000.6000
Sulfur (S)-0.0300
PhOsphorus (P)-0.0300
Nickel (Ni)1.40001.8000
Molybdenum (Mo)0.15000.3000
Manganese (Mn)1.20001.6000
Copper (Cu)-0.3000
Chromium (Cr)0.60000.9000
Carbon (C)0.50000.6000

GB/T 1299 T20102 Material Mechanical Properties

GB/T 1299 T20102 steel is an extremely versatile material due to its excellent combination of mechanical and physical properties. It has a yield strength of 390-600 MPa and tensile strength of 540-780 MPa, making it exceptionally strong and durable. It is highly resistant to deformation, offers good weldability, and is widely used in the automotive, energy and shipbuilding industry. Moreover, it is ideal for use in bridge, high-rise buildings, and structures subject to constant stress in the construction industry.

The mechanical properties of the GB/T 1299 T20102 steel are as follows:

YieldRp0.2 ≤ 773 (MPa)
TeileRm≤ 776 (MPa)
ImpactKV/Ku44(J)
ElongationA24%
Reduction in cross section on fractureZ11%
As-Heat-Treated ConditionSolution and Aging, Annealing, Ausaging, Q+T,etc
Brinell hardness (HBW)124

GB/T 1299 T20102 Material Thermal Properties

The thermal performance parameters of the GB/T 1299 T20102 steel are as follows:

Temperature (°C)21925668
Modulus of elasticity (GPa)-632-
Mean coefficient of thermal expaion ×10-6/(°C)--32
Thermal conductivity (W/m·°C)-14.312.2
Specific thermal capacity (J/kg·°C)-141-
Specific electrical resistivity (Ω mm²/m)0.34--
Deity (kg/dm³)--113
Poisson’s coefficient, ν--414