JIS G3468 SUS 316 TPY Introduce
JIS G3468 SUS 316 TPY is a type of magnetic alloy steel produced in Japan for use in a variety of industrial machinery and equipment. It is commonly used for components of manufacturing processes in machines that involve high temperatures and pressures, including motors for autos, turbines for aircraft, and pumps for industrial systems. JIS G3468 SUS 316 TPY is characterized by superior hardness, weldability, ductility, and corrosion resistance, making it an ideal material to use in demanding environments.
Smelting temperature:1424°C - 1659°C
Application:Large size welded seamless welded steel pipe
JIS G3468 SUS 316 TPY Material Chemical Composition
The chemical composition of the JIS G3468 SUS 316 TPY steel are as follows:
Element | Min | Max |
---|---|---|
Molybdenum (Mo) | 2.0000 | 3.0000 |
Nickel (Ni) | 10.0000 | 14.0000 |
Chromium (Cr) | 16.0000 | 18.0000 |
Silicon (Si) | - | 1.0000 |
Sulfur (S) | - | 0.0300 |
PhOsphorus (P) | - | 0.0450 |
Manganese (Mn) | - | 2.0000 |
Carbon (C) | - | 0.0800 |
JIS G3468 SUS 316 TPY Material Mechanical Properties
Tensile strength is a key indicator of JIS G3468 SUS 316 TPY steel's mechanical properties. This type of steel has a tensile strength range of 700 MPa - 980 MPa. The strength variability results from the different elements used in the alloy and the microstructure of the steel. For instance, adding chromium to the alloying elements increases the tensile strength of the steel. The higher the tensile strength of the material, the better its ability to withstand mechanical loads.
The mechanical properties of the JIS G3468 SUS 316 TPY steel are as follows:
YieldRp0.2 | ≤ 267 (MPa) |
TeileRm | ≤ 668 (MPa) |
ImpactKV/Ku | 13(J) |
ElongationA | 44% |
Reduction in cross section on fractureZ | 32% |
As-Heat-Treated Condition | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Brinell hardness (HBW) | 311 |
JIS G3468 SUS 316 TPY Material Thermal Properties
The thermal performance parameters of the JIS G3468 SUS 316 TPY steel are as follows:
Temperature (°C) | 41 | 398 | 935 |
Modulus of elasticity (GPa) | - | 152 | - |
Mean coefficient of thermal expaion ×10-6/(°C) | - | - | 12 |
Thermal conductivity (W/m·°C) | - | 31.3 | 32.2 |
Specific thermal capacity (J/kg·°C) | - | 224 | - |
Specific electrical resistivity (Ω mm²/m) | 0.21 | - | - |
Deity (kg/dm³) | - | - | 322 |
Poisson’s coefficient, ν | - | - | 332 |
JIS G3468 SUS 316 TPY Material Machining Technology
JIS G3468 SUS 316 TPY is one of the most important materials when it comes to machining. This type of steel is utilized for many applications, including machine parts, tools, tools and accessories, auto parts, and even architecture. JIS G3468 SUS 316 TPY steel is renowned for being an ideal steel for anything that needs precise machining and good surface finish. It has excellent machinability and thermal stability which makes it an ideal choice for many machining applications.