ASTM A582/A582M 416Se Introduce
ASTM A582/A582M 416Se is a high-strength low-alloy steel that is commonly used to manufacture components for a wide variety of industrial, commercial and residential applications. It is known for its superior chemical properties, making it a popular choice for highly corrosive environments, such as those found in coastal areas, chemical plants, and even petrochemical facilities.
Smelting temperature:1848°C - 1848°C
Application:Standard Specification for High Speed cutting Stainless Steel Bars
ASTM A582/A582M 416Se Material Chemical Composition
The chemical composition of the ASTM A582/A582M 416Se steel are as follows:
Element | Min | Max |
---|---|---|
Chromium (Cr) | 12.0000 | 14.0000 |
PhOsphorus (P) | - | 0.0600 |
Sulfur (S) | - | 0.0600 |
Manganese (Mn) | - | 1.2500 |
Silicon (Si) | - | 1.0000 |
Carbon (C) | - | 0.1500 |
ASTM A582/A582M 416Se Material Mechanical Properties
The mechanical properties of the ASTM A582/A582M 416Se steel are as follows:
YieldRp0.2 | ≤ 187 (MPa) |
TeileRm | ≤ 251 (MPa) |
ImpactKV/Ku | 24(J) |
ElongationA | 34% |
Reduction in cross section on fractureZ | 43% |
As-Heat-Treated Condition | Solution and Aging, Annealing, Ausaging, Q+T,etc |
Brinell hardness (HBW) | 223 |
ASTM A582/A582M 416Se Material Thermal Properties
The thermal performance parameters of the ASTM A582/A582M 416Se steel are as follows:
Temperature (°C) | 42 | 578 | 146 |
Modulus of elasticity (GPa) | - | 587 | - |
Mean coefficient of thermal expaion ×10-6/(°C) | - | - | 24 |
Thermal conductivity (W/m·°C) | - | 42.3 | 13.2 |
Specific thermal capacity (J/kg·°C) | - | 333 | - |
Specific electrical resistivity (Ω mm²/m) | 0.12 | - | - |
Deity (kg/dm³) | - | - | 214 |
Poisson’s coefficient, ν | - | - | 424 |